Product Details
Place of Origin: Guangdong, China
Brand Name: KangLiBang
Certification: ROHS,SGS
Payment & Shipping Terms
Minimum Order Quantity: 1KG
Price: $10-$100
Packaging Details: 1KG/bottle
Delivery Time: 5-8 work days
Payment Terms: T/T
Viscosity: |
High |
Opacity: |
Opaque |
Curing Method: |
Heat |
Flexibility: |
High |
Chemical Resistance: |
Excellent |
Abrasion Resistance: |
High |
Application Method: |
Screen Printing |
Durability: |
Long-lasting |
Temperature Resistance: |
High |
Material: |
Silicone |
Product Type: |
Ink |
Adhesion: |
Strong |
Gloss: |
Glossy |
Viscosity: |
High |
Opacity: |
Opaque |
Curing Method: |
Heat |
Flexibility: |
High |
Chemical Resistance: |
Excellent |
Abrasion Resistance: |
High |
Application Method: |
Screen Printing |
Durability: |
Long-lasting |
Temperature Resistance: |
High |
Material: |
Silicone |
Product Type: |
Ink |
Adhesion: |
Strong |
Gloss: |
Glossy |
Typical Data
Appearance |
Shallow transparent flowing liquid |
Solid Contents |
≥55% |
Viscosity |
≥10000mPa.s |
1. Engage the ready silicone rubber in second cure (190℃-200℃, 8-10minutes ), wash clean the surfaces
2. Add 3% of platinum catalyst into the silicone resin for mixture and dilute with solvent(white gas) six times ,try small quantity first followed by mass input of the solvent when diluting the silicone resin.
3. Please filtrate with 300-400 mesh filter screen for twice before uploading in the spraying gun
4. Leave alone the ready silicone resin for 3-8minutes in the dust-free plant before the spraying process.
Baking method
Baking Condition(190-200℃) 8 – 10 min
Processing |
Spray |
Spraying Viscosity (Iwata2#Cup,25℃). |
8-10 |
Spraying Distance cm |
20-25 |
Spray Mouth Diameter mm |
0.8/1.0 |
Spraying Pressure mPa |
0.2-0.3 |
Baking Condition(190-200℃)min |
8-10 |